Magnetic Permeability · CTE, linear ; 1.008 · 17.3 µm/m-°C · @Temperature 0.000 - 100 °C ; 1.008 · 9.61 µin/in-°F · @Temperature 32.0 - 212 °F. |
Specific heat capacity (0~100℃, KJ·kg-1K-1): 0.50. Thermal conductivity (W·m-1·K-1): (100℃) 16.3, (500℃) 21.5. Linear expansion coefficient (10-6·K-1): (0~100 ... |
Stainless Steel - Grade 304 (UNS S30400) ; Thermal Expansion, 16, 18 ; Breakdown Potential ; Dielectric Constant ; Resistivity, 65, 77 ... |
Thermal Expansion Coefficient. 17.3 x 10-6 °C ; Electrical Resistivity. 7.2 x 10-7 W m ; PROPERTIES RELEVANT TO SPACE USE. |
15 сент. 2022 г. · 304 stainless steel has a melting point of 1430 degrees Celius, a density of 8.00 g/cm^3, thermal expansion of 17.2x10 ^-6/K, modulus of ... |
Steel, 10.8 - 12.5. Steel Stainless Austenitic (304), 17.3. Steel Stainless Austenitic (310), 14.4. Steel Stainless Austenitic (316), 16.0. Steel Stainless ... |
The differential and mean coefficient of thermal expansion calculated from Eq. (1) are also shown in Table 8 and Table 9 Table 7 Fitting parameters of ... |
28 мар. 2023 г. · The density of 304 stainless steel is 7.93 g/cm³, and the coefficient of linear expansion is 17.2×10^-6/℃. Its thermal conductivity is 16.2 W/(m ... |