Eucalyptus Lumber Scientific Properties and Technical Specifications ; Janka Hardness: 1,125 pounds ; Strength (MOR): 16,200 psi ; Stiffness (MOE): 1,880 1000 psi ...
The Janka scale is used to determine the relative hardness of particular domestic or exotic wood species.
Janka Hardness: 1,420 lbf (6,330 N). Modulus of Rupture: 17,110 lbf/in2 ... The actual tree species, which is grown on Brazilian plantations owned by Fibria, is a ...
Eucalyptus Gummifera. 9.1. Brushbox. Tristania Conferta. 9.5. Cypress Pine. Callitris Glauca. 6.5. Grey Box. Eucalyptus Microcarpa. 15.0. Grey Iron Bark.
17 мая 2022 г. · In terms of strength and durability. Eucalyptus is considered very strong and has a high density. It is rated as moderately durable. However, ...
Janka Hardness: 1,260 lbf (5,600 N). Modulus of Rupture: 15,640 lbf/in2 (107.8 MPa). Elastic Modulus: 2,052,000 lbf/in2 (14.15 GPa). Crushing Strength: 8,020 ...
What Does The Janka Hardness Rating Mean? The Janka hardness test is the international standard for measuring the resistance of a sample of wood to denting and ...
В наличии 64. Janka Hardness: 1,260 lbf (5,600 N). Modulus of Rupture: 15,640 lbf/in2 (107.8 MPa). Elastic Modulus: 2,052,000 lbf/in2 (14.15 GPa). Crushing Strength ...