| Fiberglass & polyester | Graphite & epoxy |
Material Cost $/lb | $2.00-3.00 | $9.00-20.00+ |
Strength, yield (psi) | 30,000 | 60,000 |
Stiffness (psi) | 1.2 x 10 6 | 8 x 106 |
Density (lb/in3) | .055 | .065 |
Tensile Strength, Ultimate, 3033 MPa, 439900 psi ; Elongation at Yield, 4.8 %, 4.8 % ; Modulus of Elasticity, 69.0 GPa, 10000 ksi. |
Tensile strength varies from 28.25 MPa to 78.83 MPa, flexural strength varies from 44.65 MPa to 119.23. MPa and impact energy at room temperature varies from ... |
Used as a reinforcing agent in fiber glass composites, including biomedical/surgical applications. ... Tensile Strength, Ultimate, 4585 MPa, 665000 psi, Virgin ... |
E-Glass fibre is the most commonly used glass fibre for "fibreglass ... Tensile Strength, 1950, 2050, MPa, 282.824, 297.327, ksi. Young's Modulus, 72, 85, GPa ... |
Fiberglass offers the same strength as steel but is more flexible, making it impact-resistant. Moreover, fiberglass weighs only 25 percent of what steel does. |
21 мая 2024 г. · In most cases, higher density fiberglass means better strength and durability but could also result in a heavier end product while on the other ... |
Tensile strength: 4,600 MPa (670 ksi); Modulus of elasticity: 89 GPa (12,910 ksi); Percent elongation: 5.2. Compared to E-glass, S-fiberglass offers much higher ... |
Table 2. Comparison of glass fibre reinforced composites ; Tensile Strength. MPa. 523 ; Tensile Modulus. GPa. 23.8 ; Flexural Strength. MPa. 760 ; Flexural Modulus. |