wood hardness chart pdf - Axtarish в Google
JANKA WOOD HARDNESS RATINGS. Page 2. Hickory / Pecan, Satinwood. 1820. Afzelia / Doussie / Australian Wormy Chestnut. 1810. Bangkirai. 1798. Rosewood. 1780.
12 нояб. 2013 г. · Janka Hardness Test: A measure of the hardness of wood, produced by a variation of the Brinell Hardness. Test. The test measures the force ...
Wood Hardness Chart. Species (Alphabetical). Hardness. Species (by Hardness). Hardness. Afromosia. 1560. Basswood. 410. Amberwood. 2200. Butternut. 490.
This research study aimed to examine the wood of three deciduous wood species with low densities and great uniformity of structure.
It measures the force required to embed an 11.28mm. (.444 in) steel ball into wood to half the ball's diameter leaving an indentation in the wood. Australian ...
Janka Hardness. Rating. American White Oak. Quercus Alba. 6.0. Australian Chestnut. E. sieberi and E. obliqua. 8.0. Bamboo. 14.7 ... Janka Hardness Ratings.
A common use of Janka hardness ratings is to determine whether a species is suitable for use as flooring. The hardness of wood varies with the direction of the ...
(Ranked by Janka hardness rating). The Janka (or side) hardness test measures the force required to embed a .444-inch steel ball to half its diameter in wood.
Hardwood chart of hardness. Types of wood hardness scale. Wood ranked by hardness. The Janka hardness test is used to measure the resistance of wood to denting ...